Comparison of the Chemical Reactivity and Bioactivity of Two Bioactive Glasses 47S6 and 48S4

This work is focused on the bioactive glasses obtained by melting and rapid quenching. Two glasses with mineral composition of: 47% SiO2 - 26% CaO - 21% Na2O - 6% P2O5 and 48% SiO2 - 30% CaO - 18% Na2O - 4% P2O5 were investigated. The aim of this study was to establish the kinetics of HCAp layer for...

Full description

Saved in:
Bibliographic Details
Published in:Key engineering materials 2009-01, Vol.396-398, p.107-110
Main Authors: Mami, M., Oudadesse, Hassane, Pellen-Mussi, P., Dorbez-Sridi, R., Perez, F., Jeanne, S., Chauvel-Lebret, D., Cathelineau, G.
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:This work is focused on the bioactive glasses obtained by melting and rapid quenching. Two glasses with mineral composition of: 47% SiO2 - 26% CaO - 21% Na2O - 6% P2O5 and 48% SiO2 - 30% CaO - 18% Na2O - 4% P2O5 were investigated. The aim of this study was to establish the kinetics of HCAp layer formation “in vitro” and to control the adhesion and proliferation cells of the two glasses in contact with osseous cells. Obtained results permit to evaluate their chemical reactivity and their bioactivity after immersion in the SBF-K9. Ionic exchanges between biomaterials and SBF liquid during the “in vitro” experiments highlight the differences of the chemical reactivity and bioactivity of 47S6 and 48S4. The structural basis for the effect of cristallinity on the rates of HCA formation in vitro in favour of glasses was also established. The melt derived 47S6 and 48S4 glasses offer to surgeons new compositions with different bioactivity kinetic that bioglassÒ 45S6 and can be adaptable in some other bony pathology.