Factors on Leaching Zinc and Copper from Zinc Leach Residue

It is found that cuprous sulfite, zinc sulfate and zinc sulfide were the main phases of copper and zinc in zinc leach residue, through analyzing its composition and phase characteristics by XRF and XRD. The method that cooperate sulfuric acid leaching with oxidant was chosen. 60 g/L H2SO4 at 60 °C f...

Full description

Saved in:
Bibliographic Details
Published in:Key engineering materials 2014, Vol.633, p.169-172
Main Authors: Lang, Yao Xiu, Gao, Jun, Yang, Li Jiao, Zhong, Xia Ping, Chen, Nan Chun, Wu, Zhao Yang, Wang, Zhen Feng, Liu, Chang Miao
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:It is found that cuprous sulfite, zinc sulfate and zinc sulfide were the main phases of copper and zinc in zinc leach residue, through analyzing its composition and phase characteristics by XRF and XRD. The method that cooperate sulfuric acid leaching with oxidant was chosen. 60 g/L H2SO4 at 60 °C for 2 h with 4% KMnO4 and liquid/solid ratio of 5..1, 84.29 % of Cu and 92.02 % of Zn are extracted. The ion concentration of copper and zinc are tested by UV-VIS spectrophotometer and EDTA titration respectively. The results show that the amount of acid is sufficient for leaching at the condition of 60 g/L H2SO4 and liquid/solid ratio of 5..1. At the same time, copper change from low valence into high valence after adding KMnO4 which strengthen the leaching, and the chemical reaction can reach balance at 60 °C for 2 h. This method has good extraction effect on copper and zinc.