Loading…
Cold rolled Fe-6.5 wt. % Si alloy foils with high magnetic induction
Fe-6.5 wt. % Si alloy foils with 95 mm in width and 0.30 mm in thickness were successfully fabricated by cold rolling process. Excellent magnetic properties (Hc = 20.4 A/m, µm = 22 200, and Bs = 1.69 T) were obtained after annealing at the temperature of 1273 K for 1.5 h. This high magnetic inductio...
Saved in:
Published in: | Journal of applied physics 2012-05, Vol.111 (9) |
---|---|
Main Authors: | , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Fe-6.5 wt. % Si alloy foils with 95 mm in width and 0.30 mm in thickness were successfully fabricated by cold rolling process. Excellent magnetic properties (Hc = 20.4 A/m, µm = 22 200, and Bs = 1.69 T) were obtained after annealing at the temperature of 1273 K for 1.5 h. This high magnetic induction is considered to be due to the formation of {hk0}〈001〉 textures. Cut cores from this material have a very low iron loss at frequencies from 400 Hz to 10 kHz. |
---|---|
ISSN: | 0021-8979 1089-7550 |