Green synthesis of vanadium oxide-zirconium oxide nanocomposite for the degradation of methyl orange and picloram

The vanadium oxide-zirconium oxide nanocomposite (V2O5/ZrO2 NC) was synthesized by green method using Daphne alpine (D. alpine) leaves extract. The pore size and surface area was studied by N2 adsorption-desorption process using Brunaure-Emmett-Teller (BET) methods and SBET was found to be 214 m2 g−...

Full description

Saved in:
Bibliographic Details
Published in:Materials research express 2020-02, Vol.7 (2), p.25011
Main Authors: Rasheed, Parsa, Haq, Sirajul, Waseem, Muhammad, Rehman, Sadiq Ur, Rehman, Wajid, Bibi, Nazma, Shah, Syed Abbas Ali
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The vanadium oxide-zirconium oxide nanocomposite (V2O5/ZrO2 NC) was synthesized by green method using Daphne alpine (D. alpine) leaves extract. The pore size and surface area was studied by N2 adsorption-desorption process using Brunaure-Emmett-Teller (BET) methods and SBET was found to be 214 m2 g−1. The crystalline nature and other crystal properties was investigated by x-ray diffraction (XRD) and the calculated average crystallite size is 41.74 nm. The morphology of the V2O5/ZrO2 NC was examined by scanning electron scanning microscopy (SEM) and transmission electron microscopy (TEM). The thermal stability was examine by thermogravimetric analysis and a total of 11.73% weight loss was observed. The optical property was studied by diffuse reflectance spectroscopy (DRS) and band gap was found to be 3.93 eV. The surface function group was studied the Fourier transform infrared (FTIR) spectroscopy. The photocatalytic performance of V2O5/ZrO2 NC was examined against methyl orange and picloram and 76.94% and 86% were degraded in 75 min respectively.
ISSN:2053-1591
2053-1591
DOI:10.1088/2053-1591/ab6fa2