Cold-sintered temperature stable Na0.5Bi0.5MoO4−Li2MoO4 microwave composite ceramics

A cold sintering process (150 °C, 30 min and 200 MPa) was employed to fabricate Na0.5Bi0.5MoO4−Li2MoO4 (NBMO-LMO) composites with up to 96.4% relative density. X-ray diffraction traces, backscattered electron images and Raman spectra indicated the coexistence of NBMO and LMO phases in all composites...

Full description

Saved in:
Bibliographic Details
Main Authors: Dawei Wang, Di Zhou, Shiyu Zhang, J. C. Vardaxoglou, William Whittow, Darren Cadman, Ian M. Reaney
Format: Default Article
Published: 2017
Subjects:
Online Access:https://hdl.handle.net/2134/28035
Tags: Add Tag