Development of adhesive and cohesive failures in EVA-backsheet structures in environmental testing
The development of adhesive and cohesive failures at the EVA-backsheet interface under different damp-heat (DH) testing condition is investigated in this paper. The adhesive and cohesive failures are classified by the surface roughness of the peeled off backsheet strips. Different DH testing conditi...