The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation

To improve the damage resistance and tolerance of thin laminates manufactured with thin-ply non-crimp-fabrics, we interleaved non-woven veils into the interlaminar regions (two different types of co-polyamide veil were studied). We devised a low velocity impact and compression after impact (CAI) exp...

Full description

Saved in:
Bibliographic Details
Published in:Composites. Part A, Applied science and manufacturing Applied science and manufacturing, 2018-04, Vol.107, p.409-420
Main Authors: García-Rodríguez, S.M., Costa, J., Singery, V., Boada, I., Mayugo, J.A.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3
cites cdi_FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3
container_end_page 420
container_issue
container_start_page 409
container_title Composites. Part A, Applied science and manufacturing
container_volume 107
creator García-Rodríguez, S.M.
Costa, J.
Singery, V.
Boada, I.
Mayugo, J.A.
description To improve the damage resistance and tolerance of thin laminates manufactured with thin-ply non-crimp-fabrics, we interleaved non-woven veils into the interlaminar regions (two different types of co-polyamide veil were studied). We devised a low velocity impact and compression after impact (CAI) experimental campaign, where quasi-static indentation (QSI) tests at increasing loading displacements gave insight into the damage initiation and growth. For impact and QSI, the damage area was inspected using C-scan and X-ray micro-computed tomography. We observed that the melting temperature of the co-polyamide fibres has a key role on the impact response of thin-ply NCFs. Veils that melt during manufacturing avoided resin accumulation at the interfaces, decreased the damage area by more than 100% for a 14 J impact and improved CAI strength by up to 28%.
doi_str_mv 10.1016/j.compositesa.2018.01.023
format article
fullrecord <record><control><sourceid>csuc_cross</sourceid><recordid>TN_cdi_csuc_recercat_oai_recercat_cat_2072_324746</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S1359835X18300319</els_id><sourcerecordid>oai_recercat_cat_2072_324746</sourcerecordid><originalsourceid>FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3</originalsourceid><addsrcrecordid>eNqNkNtqGzEQhpeSQHN6B_UBdjta7UHbu2KathDITQK5E7PjkS1jS1tJNfjtI5NAe5mLYQ7w_cP_V9UXCY0EOXzdNRQOS0guc8KmBakbkA206lN1JfWo6153cFFm1U-1Vv3L5-o6pR0AKDXJq-rP05YFW8uUhfOZ457x6PxGbDGJ4EXeOl8v-5PwwdcU3WERFufoSOzx4DxmFuWGhY6cluATfxMvdcSTyOEQNhGX7akIHzllt8Hsgr-tLi3uE9-995vq-f7H0-pX_fD48_fq-0NNnYZck-pntEqOlrthQKVh7iwBEfEEQKAnreyg1zj1awQ1zwqHtutHq4apuCF1U8k3XUp_yUQmjoTZBHT_lnO1MLZGtd3YDYWZ3pkYUopszVIsYzwZCeact9mZ__I257wNSFPyLuzqjeVi6ug4mkSOPfHalX_ZrIP7gMorJiCTDA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation</title><source>ScienceDirect Journals</source><creator>García-Rodríguez, S.M. ; Costa, J. ; Singery, V. ; Boada, I. ; Mayugo, J.A.</creator><creatorcontrib>García-Rodríguez, S.M. ; Costa, J. ; Singery, V. ; Boada, I. ; Mayugo, J.A.</creatorcontrib><description>To improve the damage resistance and tolerance of thin laminates manufactured with thin-ply non-crimp-fabrics, we interleaved non-woven veils into the interlaminar regions (two different types of co-polyamide veil were studied). We devised a low velocity impact and compression after impact (CAI) experimental campaign, where quasi-static indentation (QSI) tests at increasing loading displacements gave insight into the damage initiation and growth. For impact and QSI, the damage area was inspected using C-scan and X-ray micro-computed tomography. We observed that the melting temperature of the co-polyamide fibres has a key role on the impact response of thin-ply NCFs. Veils that melt during manufacturing avoided resin accumulation at the interfaces, decreased the damage area by more than 100% for a 14 J impact and improved CAI strength by up to 28%.</description><identifier>ISSN: 1359-835X</identifier><identifier>EISSN: 1878-5840</identifier><identifier>DOI: 10.1016/j.compositesa.2018.01.023</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>B. Compression after impact ; Capes fines ; D. CT analysis ; Interleaving ; Resistència de materials ; Strength of materials ; Thin films ; Thin-ply</subject><ispartof>Composites. Part A, Applied science and manufacturing, 2018-04, Vol.107, p.409-420</ispartof><rights>2018 Elsevier Ltd</rights><rights>Tots els drets reservats info:eu-repo/semantics/openAccess</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3</citedby><cites>FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,315,786,790,891,27957,27958</link.rule.ids></links><search><creatorcontrib>García-Rodríguez, S.M.</creatorcontrib><creatorcontrib>Costa, J.</creatorcontrib><creatorcontrib>Singery, V.</creatorcontrib><creatorcontrib>Boada, I.</creatorcontrib><creatorcontrib>Mayugo, J.A.</creatorcontrib><title>The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation</title><title>Composites. Part A, Applied science and manufacturing</title><description>To improve the damage resistance and tolerance of thin laminates manufactured with thin-ply non-crimp-fabrics, we interleaved non-woven veils into the interlaminar regions (two different types of co-polyamide veil were studied). We devised a low velocity impact and compression after impact (CAI) experimental campaign, where quasi-static indentation (QSI) tests at increasing loading displacements gave insight into the damage initiation and growth. For impact and QSI, the damage area was inspected using C-scan and X-ray micro-computed tomography. We observed that the melting temperature of the co-polyamide fibres has a key role on the impact response of thin-ply NCFs. Veils that melt during manufacturing avoided resin accumulation at the interfaces, decreased the damage area by more than 100% for a 14 J impact and improved CAI strength by up to 28%.</description><subject>B. Compression after impact</subject><subject>Capes fines</subject><subject>D. CT analysis</subject><subject>Interleaving</subject><subject>Resistència de materials</subject><subject>Strength of materials</subject><subject>Thin films</subject><subject>Thin-ply</subject><issn>1359-835X</issn><issn>1878-5840</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2018</creationdate><recordtype>article</recordtype><recordid>eNqNkNtqGzEQhpeSQHN6B_UBdjta7UHbu2KathDITQK5E7PjkS1jS1tJNfjtI5NAe5mLYQ7w_cP_V9UXCY0EOXzdNRQOS0guc8KmBakbkA206lN1JfWo6153cFFm1U-1Vv3L5-o6pR0AKDXJq-rP05YFW8uUhfOZ457x6PxGbDGJ4EXeOl8v-5PwwdcU3WERFufoSOzx4DxmFuWGhY6cluATfxMvdcSTyOEQNhGX7akIHzllt8Hsgr-tLi3uE9-995vq-f7H0-pX_fD48_fq-0NNnYZck-pntEqOlrthQKVh7iwBEfEEQKAnreyg1zj1awQ1zwqHtutHq4apuCF1U8k3XUp_yUQmjoTZBHT_lnO1MLZGtd3YDYWZ3pkYUopszVIsYzwZCeact9mZ__I257wNSFPyLuzqjeVi6ug4mkSOPfHalX_ZrIP7gMorJiCTDA</recordid><startdate>201804</startdate><enddate>201804</enddate><creator>García-Rodríguez, S.M.</creator><creator>Costa, J.</creator><creator>Singery, V.</creator><creator>Boada, I.</creator><creator>Mayugo, J.A.</creator><general>Elsevier Ltd</general><general>Elsevier</general><scope>AAYXX</scope><scope>CITATION</scope><scope>XX2</scope></search><sort><creationdate>201804</creationdate><title>The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation</title><author>García-Rodríguez, S.M. ; Costa, J. ; Singery, V. ; Boada, I. ; Mayugo, J.A.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2018</creationdate><topic>B. Compression after impact</topic><topic>Capes fines</topic><topic>D. CT analysis</topic><topic>Interleaving</topic><topic>Resistència de materials</topic><topic>Strength of materials</topic><topic>Thin films</topic><topic>Thin-ply</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>García-Rodríguez, S.M.</creatorcontrib><creatorcontrib>Costa, J.</creatorcontrib><creatorcontrib>Singery, V.</creatorcontrib><creatorcontrib>Boada, I.</creatorcontrib><creatorcontrib>Mayugo, J.A.</creatorcontrib><collection>CrossRef</collection><collection>Recercat</collection><jtitle>Composites. Part A, Applied science and manufacturing</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>García-Rodríguez, S.M.</au><au>Costa, J.</au><au>Singery, V.</au><au>Boada, I.</au><au>Mayugo, J.A.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation</atitle><jtitle>Composites. Part A, Applied science and manufacturing</jtitle><date>2018-04</date><risdate>2018</risdate><volume>107</volume><spage>409</spage><epage>420</epage><pages>409-420</pages><issn>1359-835X</issn><eissn>1878-5840</eissn><abstract>To improve the damage resistance and tolerance of thin laminates manufactured with thin-ply non-crimp-fabrics, we interleaved non-woven veils into the interlaminar regions (two different types of co-polyamide veil were studied). We devised a low velocity impact and compression after impact (CAI) experimental campaign, where quasi-static indentation (QSI) tests at increasing loading displacements gave insight into the damage initiation and growth. For impact and QSI, the damage area was inspected using C-scan and X-ray micro-computed tomography. We observed that the melting temperature of the co-polyamide fibres has a key role on the impact response of thin-ply NCFs. Veils that melt during manufacturing avoided resin accumulation at the interfaces, decreased the damage area by more than 100% for a 14 J impact and improved CAI strength by up to 28%.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.compositesa.2018.01.023</doi><tpages>12</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 1359-835X
ispartof Composites. Part A, Applied science and manufacturing, 2018-04, Vol.107, p.409-420
issn 1359-835X
1878-5840
language eng
recordid cdi_csuc_recercat_oai_recercat_cat_2072_324746
source ScienceDirect Journals
subjects B. Compression after impact
Capes fines
D. CT analysis
Interleaving
Resistència de materials
Strength of materials
Thin films
Thin-ply
title The effect interleaving has on thin-ply non-crimp fabric laminate impact response: X-ray tomography investigation
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-09-21T17%3A48%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-csuc_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=The%20effect%20interleaving%20has%20on%20thin-ply%20non-crimp%20fabric%20laminate%20impact%20response:%20X-ray%20tomography%20investigation&rft.jtitle=Composites.%20Part%20A,%20Applied%20science%20and%20manufacturing&rft.au=Garc%C3%ADa-Rodr%C3%ADguez,%20S.M.&rft.date=2018-04&rft.volume=107&rft.spage=409&rft.epage=420&rft.pages=409-420&rft.issn=1359-835X&rft.eissn=1878-5840&rft_id=info:doi/10.1016/j.compositesa.2018.01.023&rft_dat=%3Ccsuc_cross%3Eoai_recercat_cat_2072_324746%3C/csuc_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c480t-c35baf317fe466a380b4fc0ccce900c08983f68da95da03bb3a62457f369fecc3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true